NPTF 7/8 Taper Socket Taper Pressure Pipe Plugs Alloy Steel B1.20.3

Dtpidbb maxb minstg
1/16"27.00000.30701/4"0.25000.23505/32"0.14000.0520
1/8"27.00000.40101/4"0.25000.23503/16"0.14000.0490
1/4"18.00000.52903/8"0.40600.39101/4"0.21800.0450
3/8"18.00000.66703/8"0.40600.39105/16"0.25000.0400
1/2"14.00000.83001/2"0.53100.51603/8"0.31200.0670
3/4"14.00001.04101/2"0.53100.51609/16"0.31200.0540
1"11.1/2.1.30205/8"0.65600.64105/8"0.37500.1120
1.1/4"11.1/2.1.64705/8"0.65600.64103/4"0.43700.1020
1.1/2"11.1/2.1.88503/4"0.65600.64103/4"0.43700.1020
Additional Info
Additional Info
Weight0.0000
MaterialALLOY STEEL
Standard NumberB1.20.3
Second Standard-
DriveHexagonsocket
HeadNON
American Generic Brand TermFLUSHSEAL
Diameter 1/16",1/8",1/4",3/8",1/2",3/4",1",1-1/4",1-1/2",2"