UNC Anco Heavy Lock Nuts Steel
UNC Anco Heavy Lock Nuts Steel
| D | D | F | F max | F min | C max | C min | H | H max | H min |
| 1/2" | 0.5000 | 7/8" | 0.875 | 0.85 | 1.01 | 0.969 | 31/64" | 0.504 | 0.464 |
| 9/16" | 0.5625 | 15/16" | 0.938 | 0.909 | 1.083 | 1.037 | 35/64" | 0.568 | 0.526 |
| 5/8" | 0.6250 | 1.1/16" | 1.062 | 1.031 | 1.227 | 1.175 | 39/64" | 0.631 | 0.587 |
| 3/4" | 0.750 | 1.1/4" | 1.250 | 1.212 | 1.443 | 1.382 | 47/64" | 0.758 | 0.710 |
| 7/8" | 0.875 | 1.7/16" | 1.438 | 1.394 | 1.66 | 1.589 | 55/64" | 0.885 | 0.833 |
| 1" | 1.000 | 1.5/8" | 1.625 | 1.575 | 1.876 | 1.796 | 63/64" | 1.012 | 0.956 |
| 1.1/8" | 1.125 | 1.13/16" | 1.812 | 1.756 | 2.093 | 2.002 | 1.7/64" | 1.139 | 1.079 |
| 1.1/4" | 1.25 | 2" | 2.000 | 1.938 | 2.309 | 2.209 | 1.7/32" | 1.251 | 1.187 |
| 1.3/8" | 1.375 | 2.3/16" | 2.188 | 2.119 | 2.526 | 2.416 | 1.11/32" | 1.378 | 1.31 |
| 1.1/2" | 1.5 | 2.3/8" | 2.375 | 2.3 | 2.742 | 2.622 | 1.15/32" | 1.505 | 1.433 |
| 1.5/8" | 1.625 | 2.9/16" | 2.562 | 2.481 | 2.959 | 2.828 | 1.19/32" | 1.632 | 1.556 |
| 1.3/4" | 1.75 | 2.3/4" | 2.750 | 2.662 | 3.175 | 3.035 | 1.23/32" | 1.759 | 1.679 |
| 1.7/8" | 1.875 | 2.15/16" | 2.938 | 2.844 | 3.392 | 3.242 | 1.27/32" | 1.886 | 1.802 |
| 2" | 2.000 | 3.1/8" | 3.125 | 3.025 | 3.608 | 3.449 | 1.31/32" | 2.013 | 1.925 |
| 2.1/4" | 2.250 | 3.1/2" | 3.500 | 3.388 | 4.041 | 3.862 | 2.13/64" | 2.251 | 2.155 |
| 2.1/2" | 2.500 | 3.7/8" | 3.875 | 3.75 | 4.474 | 4.275 | 2.29/64" | 2.505 | 2.401 |
| 2.3/4" | 2.75 | 4.1/4" | 4.250 | 4.112 | 4.907 | 4.688 | 2.45/64" | 2.759 | 2.647 |
| 3" | 3 | 4.5/8" | 4.625 | 4.475 | 5.34 | 5.102 | 2.61/64" | 3.013 | 2.893 |
| 3.1/4" | 3.25 | 5" | 5.000 | 4.838 | 5.774 | 5.515 | 3.3/16" | 3.252 | 3.124 |
| 3.1/5" | 3.5 | 5.3/8" | 5.375 | 5.2 | 6.207 | 5.928 | 3.7/16" | 3.506 | 3.370 |
| 3.3/4" | 3.75 | 5.3/4" | 5.750 | 5.562 | 6.64 | 6.341 | 3.11/16" | 3.76 | 3.616 |
| 4" | 4 | 6.1/8" | 6.125 | 5.925 | 7.073 | 6.755 | 3.15/16" | 4.014 | 3.862 |
inch UNC Anco heavy Lock Nuts Steel prevailing torque LOK MOR
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | . |
| Second Standard | - |
| Drive | Hexagon |
| Head | NON |
| American Generic Brand Term | STIFF, PREVAILING TORQUE |
| Diameter | 0 |
| Length | NON |