DDF nomF maxF minG maxG minH maxH min
No.0"0.06005/32"0.15600.15000.22100.20600.05000.0430
No.1"0.07305/32"0.15600.15000.22100.20600.05000.0430
No.2"0.08603/16"0.18800.18000.26500.24700.06600.0570
No.3"0.09903/16"0.18800.18000.26500.24700.06600.0570
No.4"0.11221/4"0.25000.24100.35400.33100.09800.0870
No.5"0.12505/16"0.31200.30200.44200.41500.11400.1020
No.6"0.13805/16"0.31200.30200.44200.41500.11400.1020
No.8"0.164011/32"0.34400.33200.48600.45600.13000.1170
No.10"0.19003/8"0.37500.36200.53000.49700.13000.1170
No.12"0.21607/16"0.43800.42300.61900.58100.16100.1480
1/4"0.25007/16"0.43800.42300.61900.58100.19300.1780
5/16"0.31259/16"0.56200.54500.79500.74800.22500.2080
3/8"0.37505/8"0.62500.60700.88400.83300.25700.2390
Additional Info
Additional Info
Weight0.0000
MaterialMild Steel A-A563
Standard NumberB18.6.3
Second Standard-
DriveSquare
HeadNON
American Generic Brand Term-
Diameter No.0",No.1",No.2",No.3",No.4",No.5",No.6",No.8",No.10",No.12",1/4",5/16",3/8"
LengthNON