Metric Coarse Square Thin Nut Stainless-Steel-A2 DIN562

SKU: 1010
Details
Details
Metric Coarse Square Thin Nut Stainless-Steel-A2 DIN562
Ds maxs mins nomem max
M1.63.20002.90003.05003.96501.0000
M24.00003.70003.85005.00501.2000
M2.55.00004.70004.85006.30501.6000
M35.50005.20005.35006.95501.8000
M3.56.00005.70005.85007.60502.0000
M47.00006.64006.82008.86602.2000
M58.00007.64007.820010.16602.7000
M610.00009.64009.820012.76603.2000
M813.000012.570012.785016.62054.0000
M1017.000016.570016.785021.82055.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A2
Standard NumberDIN562
Second Standard-
DriveSquare
HeadNON
American Generic Brand TermPRESSED
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10
LengthNON