| d | d | f max | f min | g max | g min | h max | h min | t max | t min | s max | s min |
|---|
| 1/4” | 0.250 | 0.438 | 0.428 | 0.505 | 0.488 | 0.288 | 0.274 | 0.20 | 0.18 | 0.10 | 0.07 |
| 5/16” | 0.313 | 0.500 | 0.489 | 0.577 | 0.557 | 0.336 | 0.320 | 0.24 | 0.22 | 0.12 | 0.09 |
| 3/8” | 0.375 | 0.562 | 0.551 | 0.650 | 0.628 | 0.415 | 0.398 | 0.29 | 0.27 | 0.15 | 0.12 |
| 7/16” | 0.438 | 0.688 | 0.675 | 0.794 | 0.768 | 0.463 | 0.444 | 0.31 | 0.29 | 0.15 | 0.12 |
| 1/2” | 0.500 | 0.750 | 0.736 | 0.866 | 0.840 | 0.573 | 0.552 | 0.42 | 0.40 | 0.18 | 0.15 |
| 9/16” | 0.563 | 0.875 | 0.861 | 1.010 | 0.982 | 0.621 | 0.598 | 0.43 | 0.41 | 0.18 | 0.15 |
| 5/8” | 0.625 | 0.938 | 0.922 | 1.083 | 1.051 | 0.731 | 0.706 | 0.51 | 0.49 | 0.24 | 0.18 |
| 3/4” | 0.750 | 1.125 | 1.088 | 1.299 | 1.240 | 0.827 | 0.798 | 0.57 | 0.55 | 0.24 | 0.18 |
| 7/8” | 0.875 | 1.312 | 1.269 | 1.516 | 1.447 | 0.922 | 0.890 | 0.67 | 0.64 | 0.24 | 0.18 |
| 1” | 1.000 | 1.500 | 1.450 | 1.732 | 1.653 | 1.018 | 0.982 | 0.73 | 0.70 | 0.30 | 0.24 |
| 1.1/8” | 1.125 | 1.688 | 1.631 | 1.949 | 1.859 | 1.176 | 1.136 | 0.83 | 0.80 | 0.33 | 0.24 |
| 1.1/4” | 1.250 | 1.875 | 1.812 | 2.165 | 2.066 | 1.272 | 1.228 | 0.89 | 0.86 | 0.40 | 0.31 |
| 1.3/8” | 1.375 | 2.062 | 1.994 | 2.382 | 2.273 | 1.399 | 1.351 | 1.02 | 0.98 | 0.40 | 0.31 |
| 1.1/2” | 1.500 | 2.250 | 2.175 | 2.598 | 2.480 | 1.526 | 1.474 | 1.08 | 1.04 | 0.46 | 0.37 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL |
|---|
| Standard Number | B18.2.2 |
|---|
| Second Standard | - |
|---|
| Drive | Hexagon |
|---|
| Head | Slotted |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | 0 |
|---|
| Length | NON |
|---|