UNC Slotted Hexagon Heavy Nut Steel B18.2.2 T10
SKU:
2434
Details
Details
UNC Slotted Hexagon Heavy Nut Steel B18.2.2
| d | d | f max | f min | g max | g min | h max | h min | t max | t min | s max | s min |
|---|
| 1/4” | 0.250 | 0.500 | 0.488 | 0.577 | 0.556 | 0.250 | 0.218 | 0.15 | 0.13 | 0.10 | 0.07 |
| 5/16” | 0.313 | 0.562 | 0.546 | 0.650 | 0.622 | 0.314 | 0.280 | 0.21 | 0.19 | 0.12 | 0.09 |
| 3/8” | 0.375 | 0.688 | 0.669 | 0.794 | 0.763 | 0.377 | 0.341 | 0.24 | 0.22 | 0.15 | 0.12 |
| 7/16” | 0.438 | 0.750 | 0.728 | 0.866 | 0.830 | 0.441 | 0.403 | 0.28 | 0.26 | 0.15 | 0.12 |
| 1/2” | 0.500 | 0.875 | 0.850 | 1.010 | 0.969 | 0.504 | 0.464 | 0.34 | 0.32 | 0.18 | 0.15 |
| 9/16” | 0.563 | 0.938 | 0.909 | 1.083 | 1.037 | 0.568 | 0.526 | 0.37 | 0.35 | 0.18 | 0.15 |
| 5/8” | 0.525 | 1.062 | 1.031 | 1.227 | 1.175 | 0.631 | 0.587 | 0.40 | 0.38 | 0.24 | 0.18 |
| 3/4” | 0.750 | 1.250 | 1.212 | 1.443 | 1.382 | 0.758 | 0.710 | 0.49 | 0.47 | 0.24 | 0.18 |
| 7/8” | 0.875 | 1.438 | 1.394 | 1.660 | 1.589 | 0.885 | 0.833 | 0.62 | 0.59 | 0.24 | 0.18 |
| 1” | 1.000 | 1.625 | 1.575 | 1.878 | 1.798 | 1.012 | 0.956 | 0.72 | 0.69 | 0.30 | 0.24 |
| 1.1/8” | 1.125 | 1.812 | 1.756 | 2.093 | 2.002 | 1.139 | 1.079 | 0.78 | 0.75 | 0.33 | 0.24 |
| 1.1/4” | 1.250 | 2.000 | 1.838 | 2.309 | 2.209 | 1.251 | 1.187 | 0.86 | 0.83 | 0.40 | 0.31 |
| 1.3/8” | 1.375 | 2.188 | 2.119 | 2.526 | 2.416 | 1.378 | 1.310 | 0.99 | 0.95 | 0.40 | 0.31 |
| 1.1/2” | 1.500 | 2.375 | 2.300 | 2.742 | 2.622 | 1.505 | 1.433 | 1.05 | 1.01 | 0.46 | 0.37 |
| 1.3/4” | 1.750 | 2.750 | 2.562 | 3.175 | 3.035 | 1.759 | 1.679 | 1.24 | 1.20 | 0.52 | 0.43 |
| 2” | 2.000 | 3.125 | 3.025 | 3.608 | 3.449 | 2.013 | 1.925 | 1.43 | 1.38 | 0.52 | 0.43 |
| 2.1/4” | 2.250 | 3.500 | 3.388 | 4.041 | 3.862 | 2.251 | 2.156 | 1.67 | 1.62 | 0.52 | 0.43 |
| 2.1/2” | 2.500 | 3.875 | 3.750 | 4.474 | 4.275 | 2.505 | 2.401 | 1.79 | 1.74 | 0.64 | 0.56 |
| 2.3/4” | 2.750 | 4.250 | 4.112 | 4.907 | 4.688 | 2.759 | 2.647 | 2.05 | 1.99 | 0.64 | 0.55 |
| 3” | 3.000 | 4.625 | 4.475 | 5.340 | 5.102 | 3.013 | 2.893 | 2.23 | 2.17 | 0.71 | 0.62 |
| 3.1/4” | 3.250 | 5.000 | 4.838 | 5.774 | 5.515 | 3.252 | 3.124 | 2.47 | 2.41 | 0.71 | 0.62 |
| 3.1/2” | 3.500 | 5.375 | 5.200 | 6.207 | 5.928 | 3.506 | 3.370 | 2.72 | 2.65 | 0.71 | 0.62 |
| 3.3/4” | 3.750 | 5.750 | 5.562 | 6.640 | 6.341 | 3.760 | 3.616 | 2.97 | 2.90 | 0.71 | 0.62 |
| 4” | 4.000 | 6.125 | 5.925 | 7.073 | 6.755 | 4.014 | 3.862 | 3.22 | 3.15 | 0.71 | 0.62 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL |
|---|
| Standard Number | B18.2.2 |
|---|
| Second Standard | - |
|---|
| Drive | Hexagon |
|---|
| Head | Slotted |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | 0 |
|---|
| Length | NON |
|---|