Metric Coarse Round Double Pin Nut Steel DIN547
| d | d k | m | t min | dh |
|---|
| M2 | 5.5000 | 2.0000 | 1.1000 | 2.0000 |
| M2.5 | 7.0000 | 2.2000 | 1.2000 | 2.4000 |
| M3 | 8.0000 | 2.5000 | 1.3000 | 3.0000 |
| M3.5 | 9.0000 | 3.0000 | 1.8000 | 3.0000 |
| M4 | 10.0000 | 3.5000 | 1.8000 | 3.0000 |
| M5 | 12.0000 | 4.2000 | 2.3000 | 4.0000 |
| M6 | 14.0000 | 5.0000 | 2.8000 | 5.0000 |
| M8 | 18.0000 | 6.5000 | 3.3000 | 6.0000 |
| M10 | 22.0000 | 8.0000 | 3.8000 | 7.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL |
|---|
| Standard Number | DIN547 |
|---|
| Second Standard | - |
|---|
| Drive | Hole |
|---|
| Head | ROUND |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10 |
|---|
| Length | NON |
|---|