Metric Coarse Round Double Pin Nut Stainless-Steel-A1 DIN547

SKU: 1026
Details
Details
Metric Coarse Round Double Pin Nut Stainless-Steel-A1 DIN547
dd kmt mindh
M25.50002.00001.10002.0000
M2.57.00002.20001.20002.4000
M38.00002.50001.30003.0000
M3.59.00003.00001.80003.0000
M410.00003.50001.80003.0000
M512.00004.20002.30004.0000
M614.00005.00002.80005.0000
M818.00006.50003.30006.0000
M1022.00008.00003.80007.0000
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel-A1
Standard NumberDIN547
Second Standard-
DriveHole
HeadROUND
American Generic Brand Term-
Diameter M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10