dPitchshm
M6        1          10       6.3       2.6      
M8 1.25  13  8.1  4 
M12 1.5  17  9.6  5 
M12 1.75  19  11.4  6 
M14 2  22  13  7 
M16 2  24  14.6  7.5 
M18 2.5  27  16.5  8.5 
M22 2.5  30  18.1  9.5 
M20 2.5  32  20.1  11 
M24 3  36  20.7  11.4 
M27 3  41  22.2  12.8 
M30 3.5  46  24.7  14.3 
M33 3.5  50  27.2  15.5 
M36 4  55  30  17.3 