Metric Coarse Staytite All Metal Self Locking Nut Steel

SKU: 991
Details
Details

Metric Coarse Staytite All Metal Self Locking Nut Steel

dAGHL
M478.083.803.00
M589.244.603.90
M61011.555.104.20
M81315.017.306.10
M101719.638.307.10
M121921.9410.509.00
M142225.4012.5011.00
M162427.7114.5013.00
M203034.6417.5015.40
M223236.9519.5017.20
M243641.5721.5018.80
M274147.3424.0021.20
M304653.1227.0024.00

Metric Coarse Stay tite All Metal Self Locking Nut Steel prevail

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second StandardSTAYTIGHT
DriveHexagon
HeadNON
American Generic Brand Term STIFF, PREVAILING TORQUE
Diameter0
LengthNON