ds noms macs minh nomh maxh minme
No 10.24700.25100.24300.14300.15300.13300.08100.2680
No 20.24700.25100.24300.14300.15300.13300.08100.2680
No 30.24700.25100.24300.14300.15300.13300.08100.2680
No 40.24700.25100.24300.14300.15300.13300.08100.2680
No 50.24700.25100.24300.14300.15300.13300.08100.2680
No 60.30900.31300.30500.17800.18800.16800.10300.3390
No 80.34100.34500.33600.22900.23900.21900.14000.3740
No 100.37200.37600.36700.23900.24900.22900.14000.4100
No 120.43500.43900.43000.31300.32800.29800.22500.4820
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel C3-A563
Standard Number.
Second StandardNM
DriveHexagon
HeadNON
American Generic Brand Term STIFF,PREVAILINGTORQUE
Diameter No1,No2,No3,No4,No5,No6,No8,No10,No12
LengthNON
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.