UNC Nylon Insert Self Locking NTU Thin Nut Stainless-Steel C3-A563
SKU:
904
Details
Details
UNC Nylon Insert Self Locking NTU Thin Nut Stainless-Steel C3-A563
| D | s nom | s max | s min | h nom | h max | h min | m | e |
|---|
| 1/4" | 0.4970 | 0.5020 | 0.4920 | 0.2810 | 0.2960 | 0.2660 | 0.1940 | 0.5520 |
| 5/16" | 0.5590 | 0.5640 | 0.5530 | 0.3130 | 0.3280 | 0.2980 | 0.2120 | 0.6220 |
| 3/8" | 0.6850 | 0.6900 | 0.6790 | 0.4060 | 0.4210 | 0.3910 | 0.2510 | 0.7660 |
| 7/16" | 0.7470 | 0.7520 | 0.7410 | 0.4380 | 0.4530 | 0.4230 | 0.3160 | 0.8370 |
| 1/2" | 0.8710 | 0.8770 | 0.8650 | 0.5310 | 0.5460 | 0.5160 | 0.3600 | 0.9780 |
| 9/16" | 0.9340 | 0.9400 | 0.9280 | 0.5630 | 0.5780 | 0.5480 | 0.4210 | 1.0410 |
| 5/8" | 1.0580 | 1.0640 | 1.0520 | 0.6090 | 0.6240 | 0.5940 | 0.4280 | 1.1910 |
| 3/4" | 1.2460 | 1.2520 | 1.2390 | 0.7030 | 0.7180 | 0.6880 | 0.4880 | 1.4030 |
| 7/8" | 1.4340 | 1.4400 | 1.4270 | 0.7810 | 0.7960 | 0.7660 | 0.5350 | 1.6150 |
| 1" | 1.6210 | 1.6270 | 1.6140 | 0.8910 | 0.9220 | 0.8600 | 0.6000 | 1.8070 |
| 1.1/8" | 1.8080 | 1.8140 | 1.8010 | 0.9690 | 1.0000 | 0.9380 | 0.6270 | 2.0150 |
| 1.1/4" | 1.9910 | 2.0080 | 1.9730 | 1.1090 | 1.1400 | 1.0780 | 0.7200 | 2.2190 |
| 1.3/8" | 2.1780 | 2.1970 | 2.1590 | 1.1880 | 1.2190 | 1.1570 | 0.7670 | 2.4280 |
| 1.1/2" | 2.3640 | 2.3840 | 2.3440 | 1.3130 | 1.3440 | 1.2820 | 0.8770 | 2.6360 |
| 1.3/4" | 2.7390 | 2.7620 | 2.7150 | 1.4690 | 1.5320 | 1.4060 | 0.9860 | 3.0530 |
| 2" | 3.1120 | 3.1370 | 3.0860 | 1.6720 | 1.7350 | 1.6090 | 1.0160 | 3.4690 |
| 2.1/4" | 3.5000 | 3.7800 | 3.4690 | 1.9380 | 1.8820 | 1.8270 | 1.1790 | 3.9030 |
| 2.1/2" | 4.0000 | 4.3200 | 3.9640 | 2.1870 | 2.1230 | 2.0610 | 1.5230 | 4.4600 |
| 2.3/4" | 4.0000 | 4.3200 | 3.9640 | 2.1870 | 2.1230 | 2.0610 | 1.5230 | 4.4600 |
| 3" | 4.6250 | 4.9950 | 4.5830 | 2.7250 | 2.6460 | 2.5690 | 2.0750 | 5.1570 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel C3-A563 |
|---|
| Standard Number | . |
|---|
| Second Standard | NTU |
|---|
| Drive | Hexagon |
|---|
| Head | NON |
|---|
| American Generic Brand Term | STIFF,PREVAILINGTORQUE |
|---|
| Diameter | 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2" |
|---|
| Length | NON |
|---|