| D | s max | s min | e max | h | m |
|---|
| 1/4" | 0.4450 | 0.4350 | 0.5100 | 0.2540 | 0.1230 |
| 5/16" | 0.5250 | 0.5150 | 0.6100 | 0.2940 | 0.1560 |
| 3/8" | 0.6000 | 0.5850 | 0.6900 | 0.3330 | 0.1980 |
| 7/16" | 0.7100 | 0.6950 | 0.8200 | 0.4030 | 0.2400 |
| 1/2" | 0.8200 | 0.8000 | 0.9500 | 0.4470 | 0.2810 |
| 5/8" | 1.0100 | 0.9850 | 1.1700 | 0.5350 | 0.3650 |
| 3/4" | 1.2000 | 1.1750 | 1.3900 | 0.7310 | 0.4480 |
| 7/8" | 1.3000 | 1.2700 | 1.5000 | 0.7620 | 0.4900 |
| 1" | 1.4800 | 1.4500 | 1.7100 | 0.8210 | 0.5730 |
| 1.1/8" | 1.6700 | 1.6400 | 1.9300 | 0.9050 | 0.6560 |
| 1.1/4" | 1.8600 | 1.8150 | 2.1500 | 1.0650 | 0.7300 |
| 1.1/2" | 2.2200 | 2.1750 | 2.5600 | 1.2740 | 0.8960 |
| 1.3/4" | 2.5800 | 2.5200 | 2.9800 | 1.4500 | 1.0630 |
| 2" | 2.7600 | 2.7000 | 3.1900 | 1.5650 | 1.1460 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL |
|---|
| Standard Number | . |
|---|
| Second Standard | - |
|---|
| Drive | Hexagon |
|---|
| Head | NON |
|---|
| American Generic Brand Term | STIFF,PREVAILINGTORQUE |
|---|
| Diameter | 3/16",1/4",5/16",3/8",7/16",1/2",5/8",3/4",7/8",1",1.1/8",1.1/4",1.1/2",1.3/4",2" |
|---|
| Length | NON |
|---|