BSW Whitworth Oval Neck Cup Head Bolts Grade-4.6 BS325
BSW Whitworth Oval Neck Cup Head Bolts Grade-4.6 BS325
d | 3/4" | 7/8" |
A | 1.688 | 1.969 |
B | 0.438 | 0.500 |
C | 1/16" | 3/32" |
R | 3/64" | 1/16" |
E | 0.625 | 0.625 |
F | 1.000 | 1.125 |
G | 0.375 | 0.438 |
H | 0.250 | 0.250 |
BSW Whitworth Oval Neck Cup Head Bolts Grade- 4.6 BS 325 TABLE 2
Weight | 0.0000 |
---|---|
Material | Grade-4.6 |
Standard Number | BS325 |
Second Standard | - |
Drive | - |
Head | - |
American Generic Brand Term | OVAL |
Diameter | 0 |
Length | 0 |