| Thread | A | A1 | B | C | D | F | T |
| No10 Unc | 0.6875 | 0.7031 | 0.2813 | 0.243 | 0.2188 | 0.3125 | 0.039 |
| No10 Unc | 0.6875 | 0.7031 | 0.3125 | 0.243 | 0.2500 | 0.3281 | 0.039 |
| No10 Unf | 0.6875 | 0.7031 | 0.2813 | 0.243 | 0.2188 | 0.3125 | 0.039 |
| No10 Unf | 0.6875 | 0.7031 | 0.4375 | 0.243 | 0.3125 | 0.2969 | 0.039 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.2500 | 0.305 | 0.2188 | 0.3281 | 0.047 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.2500 | 0.305 | 0.1875 | 0.3350 | 0.047 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.3125 | 0.305 | 0.2344 | 0.3350 | 0.047 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.3750 | 0.305 | 0.3125 | 0.3350 | 0.047 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.4375 | 0.305 | 0.3125 | 0.3350 | 0.047 |
| 1/4 Unc | 0.6875 | 0.7031 | 0.5625 | 0.305 | 0.2969 | 0.3350 | 0.047 |
| 5/16 Unc | 0.8281 | 0.8125 | 0.3750 | 0.370 | 0.3125 | 0.4090 | 0.051 |
| 5/16 Unc | 0.8281 | 0.8125 | 0.6250 | 0.370 | 0.3750 | 0.4090 | 0.051 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | . |
| Second Standard | - |
| Drive | - |
| Head | - |
| American Generic Brand Term | - |
| Diameter | 0 |
| Length | NON |