Inch Unc Sealing Nut
| Size | A Max | A Min | B Max | B Min | C |
| No 2 | 0.1880 | 0.1800 | 0.2170 | 0.2050 | 0.0615 |
| No 4 | 0.2500 | 0.2410 | 0.2890 | 0.2750 | 0.0925 |
| No 6 | 0.3120 | 0.3020 | 0.3610 | 0.3440 | 0.1080 |
| No 8 | 0.3440 | 0.3320 | 0.3970 | 0.3780 | 0.1235 |
| No 10 | 0.3750 | 0.3620 | 0.4330 | 0.4130 | 0.1235 |
| 1/4" | 0.5000 | 0.4880 | 0.5770 | 0.5560 | 0.2340 |
| 5/16" | 0.5620 | 0.5460 | 0.6500 | 0.6220 | 0.2960 |
| 3/8" | 0.6880 | 0.6690 | 0.7940 | 0.7630 | 0.3590 |
| 7/16" | 0.7500 | 0.7280 | 0.8660 | 0.8300 | 0.4210 |
| 1/2" | 0.8750 | 0.8500 | 1.0100 | 0.9690 | 0.4840 |
| 9/16" | 0.9380 | 0.9090 | 1.0830 | 1.0370 | 0.5460 |
| 5/8" | 1.0620 | 1.0310 | 1.2270 | 1.1750 | 0.6090 |
| 3/4" | 1.2500 | 1.2120 | 1.4430 | 1.3820 | 0.7340 |
| 7/8" | 1.4380 | 1.3940 | 1.6600 | 1.5890 | 0.8590 |
| 1" | 1.6250 | 1.5750 | 1.8760 | 1.7960 | 0.9840 |
Inch Unc Sealing Nut
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | GRADE 2 AND GRADE 5 AND STAINLESS STEEL |
| Second Standard | - |
| Drive | Hexagon |
| Head | - |
| American Generic Brand Term | - |
| Diameter | SEE TABLE |
| Length | . |