UNC Cage Nut Stainless-Steel
SKU:
1054
Details
Details
UNC Cage Nut Stainless-Steel
| d | P | A | F | G | sq hole | hole r |
|---|
| 1/4UNC | 0.7/1.6 | 13.5000 | 13.5000 | 5.8000 | 9.5000 | 0.8000 |
| 1/4UNC | 0.7/2.0 | 13.5000 | 13.5000 | 6.0000 | 9.5000 | 0.8000 |
| 1/4UNC | 0.7/2.1 | 13.5000 | 13.5000 | 6.5000 | 9.5000 | 0.8000 |
| 1/4UNC | 1.8/2.6 | 13.5000 | 13.5000 | 5.8000 | 9.5000 | 0.8000 |
| 1/4UNC | 2.1/3.0 | 13.5000 | 13.5000 | 6.0000 | 9.5000 | 0.8000 |
| 1/4UNC | 2.2/3.1 | 13.5000 | 13.5000 | 6.5000 | 9.5000 | 0.8000 |
| 5/16UNC | 0.7/1.6 | 17.8000 | 18.0000 | 7.2000 | 12.8000 | 3.2000 |
| 5/16UNC | 1.8/2.6 | 17.8000 | 18.0000 | 7.2000 | 12.8000 | 3.2000 |
| 3/8UNC | 0.7/1.6 | 17.8000 | 18.0000 | 7.2000 | 12.8000 | 3.2000 |
| 3/8UNC | 1.8/2.6 | 17.8000 | 18.0000 | 7.2000 | 12.8000 | 3.2000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel |
|---|
| Standard Number | . |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | NON |
|---|
| American Generic Brand Term | PANEL,CAPTIVE |
|---|
| Diameter | 1/4",5/16",3/8" |
|---|
| Length | NON |
|---|