Metric Coarse Knurled Flange Nut Steel DIN193
| D | d1 | s | m |
|---|---|---|---|
| M5 | 11.2000 | 8.0000 | 4.3000 |
| M6 | 14.2000 | 10.0000 | 5.5000 |
| M8 | 18.2000 | 13.0000 | 7.0000 |
| M10 | 21.0000 | 15.0000 | 8.5000 |
| M12 | 24.0000 | 17.0000 | 10.0000 |
| M16 | 31.0000 | 22.0000 | 14.0000 |
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | DIN193 |
| Second Standard | - |
| Drive | Hexagon |
| Head | - |
| American Generic Brand Term | - |
| Diameter | M5,M6,M8,M10,M12,M16 |
| Length | NON |