Metric Coarse Binx Nut Stainless-Steel-A2
Metric Coarse Binx Nut Stainless Steel A2
| D | S | h |
|---|---|---|
| M3 | 5.5000 | 3.2000 |
| M4 | 7.0000 | 3.2000 |
| M5 | 8.0000 | 4.1000 |
| M6 | 10.0000 | 6.1000 |
| M8 | 13.0000 | 6.4000 |
| M10 | 17.0000 | 7.9000 |
| M12 | 19.0000 | 9.9000 |
| M14 | 22.0000 | 11.0000 |
| M16 | 24.0000 | 13.0000 |
| M18 | 27.0000 | 15.0000 |
| M20 | 30.0000 | 16.0000 |
| M22 | 32.0000 | 17.8000 |
| M24 | 36.0000 | 18.8000 |
| M27 | 41.0000 | 22.2000 |
| M30 | 46.0000 | 23.9000 |
| M36 | 55.0000 | 32.0000 |
Metric Coarse Binx Nut Stainless Steel A2 all metal lock locking bent beam
| Weight | 0.0000 |
|---|---|
| Material | Stainless-Steel-A2 |
| Standard Number | . |
| Second Standard | BINX |
| Drive | Hexagon |
| Head | NON |
| American Generic Brand Term | STIFF, PREVAILING TORQUE |
| Diameter | M3,M4,M5,M6,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M36 |
| Length | NON |