Metric Coarse All Metal Self Locking Nut with Flange Class-8 DIN6927
Metric Coarse All Metal Self Locking Nut with Flange Class-8 DIN6927
| d | h | m | dc | e | s | c |
|---|---|---|---|---|---|---|
| ?5 | 6.2000 | 4.7000 | 11.8000 | 8.7900 | 8.0000 | 1.0000 |
| M6 | 7.3000 | 5.7000 | 14.2000 | 11.0500 | 10.0000 | 1.1000 |
| M8 | 9.4000 | 7.6000 | 17.9000 | 14.3800 | 13.0000 | 1.2000 |
| M10 | 11.4000 | 9.6000 | 21.8000 | 17.7700 | 16.0000 | 1.5000 |
| M12 | 13.8000 | 11.6000 | 26.0000 | 20.0300 | 18.0000 | 1.8000 |
| M14 | 15.9000 | 13.3000 | 29.9000 | 23.3600 | 21.0000 | 2.1000 |
| M16 | 18.3000 | 15.3000 | 34.5000 | 26.7500 | 24.0000 | 2.4000 |
| ?20 | 22.4000 | 18.7000 | 42.8000 | 32.9500 | 30.0000 | 2.9000 |
| Weight | 0.0000 |
|---|---|
| Material | Class-8 |
| Standard Number | DIN6927 |
| Second Standard | ISO7044 |
| Drive | Hexagon |
| Head | NON |
| American Generic Brand Term | STIFF, PREVAILING TORQUE |
| Diameter | ?5,M6,M8,M10,M12,M14,M16,?20 |
| Length | NON |