Metric Coarse Structural Hexagon Full Nut HSFG Class-10 BS EN15048 Non Preload
Metric Coarse Structural Hexagon Full Nut HSFG Class-10 BS EN15048
| d | M12 | M16 | M20 | M24 | M30 | M36 |
| da max | 13.00 | 17.30 | 21.60 | 25.90 | 32.40 | 38.90 |
| da min | 12.00 | 16.00 | 20.00 | 24.00 | 30.00 | 36.00 |
| dw min | 16.60 | 22.50 | 27.70 | 33.30 | 42.80 | 51.10 |
| e min | 20.03 | 26.75 | 32.95 | 39.55 | 50.85 | 60.79 |
| m max | 10.80 | 14.80 | 18.00 | 21.50 | 25.60 | 31.00 |
| m min | 10.37 | 14.10 | 16.90 | 20.20 | 24.30 | 29.40 |
| s max | 18.00 | 24.00 | 30.00 | 36.00 | 46.00 | 55.00 |
| s min | 17.73 | 23.67 | 29.16 | 35.00 | 45.00 | 53.80 |
Metric Coarse Structural Hexagon Full Nut H.S.F.G Class 10 BS EN5048
| Weight | 0.0000 |
|---|---|
| Material | Class-10 |
| Standard Number | EN143993 |
| Second Standard | - |
| Drive | Hexagon |
| Head | NON |
| American Generic Brand Term | HIGHSTRENGTHFRICTIONGRIPNUT |
| Diameter | M12,M16,M20,M22,M24,M27,M30,M36 |
| Length | NON |