UNC Hexagon Lock Nut SAE-8(10.9) B18.2.2

SKU: 733
Details
Details
UNC Hexagon Lock Nut SAE-8(10.9) B18.2.2
DDss maxs mine maxe minmm maxm min
1/4"0.25007/16"0.43800.42800.50500.48805/32"0.16300.1500
5/16"0.31251/2"0.50000.48900.57700.55703/16"0.19500.1800
3/8"0.37509/16"0.56200.55100.65000.62807/32"0.22700.2100
7/16"0.437511/16"0.68800.67500.79400.76801/4"0.26000.2400
1/2"0.50003/4"0.75000.73600.86600.84005/16"0.32300.3020
9/16"0.56257/8"0.87500.86101.01000.98205/16"0.32400.3010
5/8"0.625015/16"0.93800.92201.08301.05103/8"0.38700.3630
3/4"0.75001.1/8"1.12501.08801.29901.240027/64"0.44600.3980
7/8"0.87501.5/16"1.31201.26901.51601.447031/64"0.51000.4580
1"1.00001.1/2"1.50001.45001.73201.653035/64"0.57500.5190
1.1/8"1.12501.11/16"1.68801.63101.94901.859039/64"0.63900.5790
1.1/4"1.25001.7/8"1.87501.81202.16502.066023/32"0.75100.6870
1.3/8"1.37502.1/16"2.06201.99402.38202.273025/32"0.81500.7470
1.1/2"1.50002.1/4"2.25002.17502.59802.480027/32"0.88000.8080
Additional Info
Additional Info
Weight0.0000
MaterialSAE-8(10.9)
Standard NumberB18.2.2
Second StandardBS1768
DriveHexagon
HeadNON
American Generic Brand TermJAMNUT.HALFNUT
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2"
LengthNON