d e s max s min m max m min
1/4"0.51000.44500.43800.13300.1230
5/16"0.61000.52500.51800.16600.1560
3/8"0.69000.60000.59200.20800.1980
7/16"0.82000.71000.70200.25000.2400
1/2"0.95000.82000.81200.29100.2810
9/16"1.06000.92000.91200.33300.3230
5/8"1.17001.01001.00000.37500.3650
3/4"1.39001.20001.19000.45800.4480
7/8"1.50001.30001.28800.50000.4900
1"1.71001.48001.46800.58300.5730
1.1/8"1.93001.67001.64000.66600.6560
1.1/4"2.15001.86001.81500.75000.7300
1.3/8"2.37002.05002.00500.83300.8130
1.1/2"2.56002.22002.17500.91600.8960
1.3/4"2.98002.58002.52001.08301.0630
2"3.19002.76002.70001.16601.1460
Additional Info
Additional Info
Weight0.0000
MaterialStainless-Steel
Standard NumberBS1083
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermHALFNUT,JAMNUT
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.3/4",2.
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.