DDss maxs mine maxe minmm maxm min
1/4"0.25001/2"0.50000.48800.57700.556011/64"0.18800.1560
5/16"0.31259/16"0.56200.54600.65000.622013/64"0.22000.1860
3/8"0.375011/16"0.68800.66900.79400.763015/64"0.25200.2160
7/16"0.43753/4"0.75000.72800.86600.830017/64"0.28500.2470
1/2"0.50007/8"0.87500.85001.01000.969019/64"0.31700.2770
9/16"0.562515/16"0.93800.90901.08301.037021/64"0.34900.3070
5/8"0.62501.1/16"1.06201.03101.22701.175023/64"0.38100.3370
3/4"0.75001.1/4"1.25001.21201.44301.382027/64"0.44600.3980
7/8"0.87501.7/16"1.43801.39401.66001.589031/64"0.51000.4580
1"1.00001.5/8"1.62501.57501.87601.796035/64"0.57500.5190
1.1/8"1.12501.13/16"1.81201.75602.09302.002039/64"0.63900.5790
1.1/4"1.25002"2.00001.93802.30902.209023/32"0.75100.6870
1.3/8"1.37502.3/16"2.18802.11902.52602.416025/32"0.81500.7470
1.1/2"1.50002.3/8"2.37502.30002.74202.622027/32"0.88000.8080
1.5/8"1.62502.9/16"2.56202.48102.95902.828029/32"0.94400.8680
1.3/4"1.75002.3/4"2.75002.66203.17503.035031/32"1.00900.9290
1.7/8"1.87502.15/16"2.93802.84403.39203.24201.1/32"1.07300.9890
2"2.00003.1/8"3.12503.02503.60803.44901.3/32"1.13801.0500
2.1/4"2.25003.1/2"3.50003.38804.04103.86201.13/64"1.25101.1550
2.1/2"2.50003.7/8"3.87503.75004.47404.27501.29/64"1.50501.4010
2.3/4"2.75004.1/4"4.25004.11204.90704.68801.37/64"1.63401.5220
3"3.00004.5/8"4.62504.47505.34005.10201.45/64"1.76301.6430
3.1/4"3.25005"5.00004.83805.77405.51501.13/16"1.87601.7480
3.1/5"3.50005.3/8"5.37505.20006.20705.92801.15/16"2.00601.8700
3.3/4"3.75005.3/4"5.75005.56206.64006.34102.1/16"2.13401.9900
4"4.00006.1/8"6.12505.92507.07306.75502.3/16"2.26402.1120
Additional Info
Additional Info
Weight0.0000
MaterialMild Steel A-A563
Standard NumberB18.2.2
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermJAMNUT.HALFNUT
Diameter 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",1.7/8",2",2.1/4",2.1/2",2.3/4",3",3.1/4",3.1/5",3.3/4",4"
LengthNON
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.