Metric Coarse Serrated Hexagon Flange Nut Durlok Steel Class 12
Metric Coarse Serrated Hexagon Flange Nut Durlok Steel
| d | d | d1 min | d2 | e min | k | k1 max | k2 | S |
|---|---|---|---|---|---|---|---|---|
| M5 | 12.00 | 10.00 | 6.20 | 8.84 | 4.50 | 2.17 | 1.00 | 8.00 |
| M6 | 14.00 | 11.80 | 7.40 | 11.10 | 5.20 | 2.27 | 1.10 | 10.00 |
| M8 | 18.00 | 15.20 | 9.50 | 14.49 | 7.20 | 2.70 | 1.30 | 13.00 |
| M10 | 21.00 | 17.20 | 12.50 | 16.64 | 9.00 | 3.24 | 1.60 | 15.00 |
| M12 | 25.00 | 20.60 | 15.00 | 21.10 | 11.00 | 4.00 | 1.90 | 19.00 |
| M14 | 28.00 | 22.80 | 17.00 | 24.50 | 12.50 | 4.50 | 2.20 | 22.00 |
| M16 | 32.00 | 25.70 | 19.00 | 26.80 | 14.50 | 3.90 | 2.40 | 24.00 |
| M20 | 39.00 | 31.20 | 22.30 | 34.00 | 18.00 | 4.00 | 2.40 | 30.00 |
The Durlok® self-locking system is the solution to one of the most persistent problems in the field of fastener technology.
VIBRATION.
Durlok nuts and bolts will not loosen or unscrew even under the most severe transverse jarring and vibration.
The Durlok fastener system is effective on a wide variety of engineering materials including steel -- both heat-treated and non heat-treated, cast irons including nodular types, non-ferrous metals and sheet materials.
Durlok nuts and bolts are suitable for re-use because the serrations cause relatively little damage to the clamped material.
durlock derlock
| Weight | 0.0000 |
|---|---|
| Material | STEEL |
| Standard Number | . |
| Second Standard | DURLOCK |
| Drive | Hexagon |
| Head | Flange |
| American Generic Brand Term | - |
| Diameter | M5 to M20 |
| Length | No |