Metric Coarse Hexagon Flange Nut Stainless-Steel-A2 DIN6923
| d | dc | s | m | C |
|---|
| M3 | 8.0000 | 5.5000 | 3.7000 | |
| M4 | 10.0000 | 7.0000 | 4.5000 | |
| M5 | 11.8000 | 8.0000 | 5.0000 | |
| M6 | 14.2000 | 10.0000 | 6.0000 | |
| M8 | 17.9000 | 13.0000 | 8.0000 | |
| M10 | 21.8000 | 15.0000 | 10.0000 | |
| M12 | 26.0000 | 18.0000 | 12.0000 | |
| M14 | 29.9000 | 21.0000 | 14.0000 | |
| M16 | 34.5000 | 24.0000 | 16.0000 | |
| M20 | 42.8000 | 30.0000 | 20.0000 | |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A2 |
|---|
| Standard Number | DIN6923 |
|---|
| Second Standard | ISO4161 |
|---|
| Drive | Hexagon |
|---|
| Head | Flange |
|---|
| American Generic Brand Term | - |
|---|
| Diameter | M3,M4,M5,M6,M8,M10,M12,M14,M16,M20,M24 |
|---|
| Length | NON |
|---|