d         e      s max   s min          m
1/4"0.510.450.440.60
5/16"0.610.530.520.75
3/8"0.690.600.590.94
7/16"0.820.710.701.13
1/2"0.950.820.811.31
9/16"1.060.920.911.50
5/8"1.171.011.001.69
3/4"1.391.201.192.06
7/8"1.501.301.292.25
1"1.711.481.472.63
1.1/8"1.931.671.643.00
1.1/4"2.151.861.823.38
1.3/8"2.372.052.013.75
1.1/2"2.562.222.184.13
1.3/4"2.982.582.524.88
2"3.192.762.705.25

 

 

studding allthread connector nut

Additional Info
Additional Info
Weight0.0000
MaterialBRASS