Metric Coarse Engineers Stud Slotted Brass DIN427

SKU: 1975
Details
Details
Metric Coarse Engineers Stud Slotted Brass DIN427
d1bnt
M11.20000.26000.4000
M1.21.40000.26000.4000
M1.41.70000.26000.4800
M1.61.90000.31000.5600
M22.40000.31000.6400
M2.53.00000.46000.7200
M33.60000.46000.8000
M3.54.20000.56000.9600
M44.80000.66001.1200
M56.00000.86001.2800
M67.20001.06001.6000
M89.60001.26002.0000
M1012.00001.66002.4000
M1214.00002.06002.8000
M1416.00002.06003.2000
M1618.00002.56003.2000
M1820.00003.06004.0000
M2022.00003.06004.0000
Additional Info
Additional Info
Weight0.0000
MaterialBRASS
Standard NumberDIN427
Second StandardISO2342
DriveSlot
HeadNON
American Generic Brand Term-
Diameter M1,M1.2,M1.4,M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M8,M10,M12,M14,M16,M18,M20
Length2.5,3,4,5,6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60