UNC 12 Point Flange Head Bolt SAE-5(8.8) SAEJ58
| D | ds | dc max | dc min | dk max | dk min | h | k | b |
|---|---|---|---|---|---|---|---|---|
| 1/4” | 0.2435 | 0.3750 | 0.3650 | 0.2520 | 0.2440 | 0.0580 | 0.2600 | 1.0000 |
| 5/16” | 0.3053 | 0.4690 | 0.4570 | 0.3150 | 0.3060 | 0.0740 | 0.3120 | 1.1250 |
| 3/8” | 0.3678 | 0.5620 | 0.5500 | 0.3770 | 0.3680 | 0.0950 | 0.3750 | 1.2500 |
| 7/16” | 0.4294 | 0.6560 | 0.6420 | 0.4380 | 0.4280 | 0.1090 | 0.4380 | 1.3750 |
| 1/2” | 0.4919 | 0.7500 | 0.7350 | 0.5020 | 0.4930 | 0.1290 | 0.5000 | 1.5000 |
| 9/16” | 0.5538 | 0.8440 | 0.8280 | 0.5640 | 0.5550 | 0.1450 | 0.5630 | 1.6250 |
| 5/8” | 0.6163 | 0.9380 | 0.9210 | 0.6270 | 0.6180 | 0.1660 | 0.6250 | 1.7500 |
| 3/4” | 0.7406 | 1.1250 | 1.1070 | 0.7520 | 0.7430 | 0.2000 | 0.7500 | 2.0000 |
| 7/8” | 0.8647 | 1.3120 | 1.2930 | 0.8770 | 0.8660 | 0.2340 | 0.8750 | 2.2500 |
| 1” | 0.9886 | 1.5000 | 1.4790 | 1.0030 | 0.9910 | 0.2680 | 1.0000 | 2.5000 |
| 1.1/8” | 1.1086 | 1.6880 | 1.6650 | 1.1280 | 1.1150 | 0.3100 | 1.1250 | 2.7500 |
| 1.1/4” | 1.2335 | 1.8750 | 1.8520 | 1.2530 | 1.2400 | 0.3500 | 1.2500 | 3.0000 |
| 1.3/8” | 1.3568 | 2.0620 | 2.0380 | 1.3780 | 1.3650 | 0.3920 | 1.3750 | 3.2500 |
| 1.1/2” | 1.4818 | 2.2500 | 2.2240 | 1.5030 | 1.4890 | 0.4330 | 1.5000 | 3.5000 |
| Weight | 0.0000 |
|---|---|
| Material | SAE-5(8.8) |
| Standard Number | SAEJ58 |
| Second Standard | - |
| Drive | 12point |
| Head | Flange |
| American Generic Brand Term | FERRY |
| Diameter | 1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2" |
| Length | 1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6.",6.1/2",7.",7.1/2",8 |