Metric Coarse Indented Foundation Bolt Grade-3.6 DIN529E

SKU: 167
Details
Details
Metric Coarse Indented Foundation Bolt Grade-3.6 DIN529E
dac
M816.000045.0000
M1020.000055.0000
M1224.000070.0000
M1632.000090.0000
M2040.0000100.0000
M2448.0000135.0000
M3060.0000150.0000
M3672.0000180.0000
M4285.0000260.0000
M4898.0000260.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-3.6
Standard NumberDIN529E
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter M6,M8,M10,M12,M16
Length24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100