Metric Coarse 12 Point Spline Bell Flange Head Bolt Grade-10.9 B18.2.7.1M
SKU:
113
Details
Details
Metric Coarse 12 Point Spline Bell Flange Head Bolt Grade-10.9 B18.2.7.1M
| D | b | ds max | ds min | dc max | k max |
|---|
| M5 | 16.0000 | 5.0000 | 4.8200 | 9.4000 | 5.0000 |
| M6 | 18.0000 | 6.0000 | 5.8200 | 11.3000 | 6.0000 |
| M8 | 22.0000 | 8.0000 | 7.7800 | 15.0000 | 8.0000 |
| M10 | 26.0000 | 10.0000 | 9.7800 | 18.6000 | 10.0000 |
| M12 | 30.0000 | 12.0000 | 11.7300 | 22.8000 | 12.0000 |
| M14 | 34.0000 | 14.0000 | 13.7300 | 26.4000 | 14.0000 |
| M16 | 38.0000 | 16.0000 | 15.7300 | 30.3000 | 16.0000 |
| M20 | 46.0000 | 20.0000 | 19.6700 | 37.4000 | 20.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Grade-10.9 |
|---|
| Standard Number | B18.2.7.1M |
|---|
| Second Standard | - |
|---|
| Drive | 12point |
|---|
| Head | Flange |
|---|
| American Generic Brand Term | SPLINE,FERRY,BELL |
|---|
| Diameter | M5,M6,M8,M10,M12,M14,M16,M20 |
|---|
| Length | 16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100 |
|---|