WIREABCDEFGH
1/8"0.22000.72000.44000.47000.37000.38000.81000.9900
3/16"0.25000.97000.56000.59000.50000.44000.94001.1800
1/4"0.31001.03000.50000.75000.66000.56001.19001.4300
5/16"0.38001.38000.75000.88000.73000.69001.31001.6600
3/8"0.44001.50000.75001.00000.91000.75001.63001.9400
7/16"0.50001.88001.00001.19001.13000.88001.91002.2800
1/2"0.50001.88001.00001.19001.13000.88001.91002.2800
9/16"0.56002.25001.25001.31001.34000.94002.06002.5000
5/8"0.56002.25001.25001.31001.34000.94002.06002.5000
3/4"0.62002.75001.44001.50001.39001.06002.25002.8400
7/8"0.75003.12001.62001.75001.58001.25002.44003.1600
1"0.75003.50001.81001.88001.77001.25002.63003.4700
1.1/8"0.75003.88002.00002.00001.91001.25002.81003.5900
1.1/4"0.88004.44002.22002.34002.17001.44003.13004.1300
1.3/8"0.88004.44002.22002.34002.31001.44003.13004.1900
1.1/2"0.88004.94002.38002.59002.44001.44003.41004.4400
1.5/8"1.00005.31002.62002.75002.66001.63003.63004.7500
1.3/4"1.13005.75002.75003.06002.92001.81003.81005.2400
2."1.25006.44003.00003.38003.03002.00004.44005.8800
2.1/4"1.25007.13003.19003.88003.19002.00004.56006.3800
2.1/2"1.25007.69003.44004.13003.69002.00004.69006.6300
2.3/4"1.25008.31003.56004.38004.88002.00005.00006.8800
3."1.50009.19003.88004.75004.44002.38005.31007.6100
3.1/2"1.500010.75004.50005.50006.00002.38006.19008.3800
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberUSA
Second Standard-
DriveNon
HeadNON
American Generic Brand Term-
Diameter 1/8",3/16",1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4",7/8",1",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.1/2",2.3/4",3.",3.1/2"
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.