DetailsMetric Coarse Oval Neck Mine Bolts Steel DIN21547 DIN 21547
| d | b less than 75 | b between 75 160 | b more than 160 | f max | f min | e max | e min | h max | h min | m max | m min |
|---|
| M20 | 45 | 60 | 70 | 38.80 | 37.20 | 20.00 | 19.67 | 13.40 | 11.60 | 8.00 | 7.60 |
| M24 | 45 | 60 | 70 | 42.80 | 41.20 | 24.00 | 23.67 | 16.90 | 15.10 | 10.00 | 9.60 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | STEEL |
|---|
| Standard Number | DIN21547 |
|---|
| Second Standard | - |
|---|
| Drive | - |
|---|
| Head | - |
|---|
| American Generic Brand Term | ROUND HEAD BOLTS WITH OVAL SHOULDER |
|---|
| Diameter | 0 |
|---|
| Length | 0 |
|---|