Metric Coarse Elevator Bucket Bolt Stainless-Steel 18/8-304-A2 DIN15237
SKU:
225
Details
Details
Metric Coarse Elevator Bucket Bolt Stainless-Steel 18/8-304-A2 DIN15237
| d | k | g | a | d3 |
|---|
| M6 | 2.5000 | 3.5000 | 14.0000 | 20.0000 |
| M8 | 3.5000 | 5.0000 | 20.0000 | 28.0000 |
| M 10 | 4.5000 | 6.0000 | 25.0000 | 35.0000 |
| M 12 | 5.2000 | 7.0000 | 30.0000 | 42.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel 18/8-304-A2 |
|---|
| Standard Number | DIN15237 |
|---|
| Second Standard | - |
|---|
| Drive | Non |
|---|
| Head | Dish |
|---|
| American Generic Brand Term | SEATING SCREW |
|---|
| Diameter | M6,M7,M8,M10,M12 |
|---|
| Length | 20,22,24,26,28,30,35,40,45,50,55,60,65,70 |
|---|