Metric Coarse Countersunk Short Square Neck Bolt Grade-8.8 DIN608
| d | a | f | dk | v max | v min |
|---|---|---|---|---|---|
| M10 | 90° | 8.4500 | 19.6500 | 10.5800 | 9.4200 |
| M12 | 90° | 11.0500 | 24.6500 | 12.7000 | 11.3000 |
| Weight | 0.0000 |
|---|---|
| Material | Grade-8.8 |
| Standard Number | DIN608 |
| Second Standard | - |
| Drive | Square |
| Head | COUNTERSUNK |
| American Generic Brand Term | FLAT |
| Diameter | M10,M12 |
| Length | 25,26,28,30,35,40,45,50 |