UNC Blind Bolt Steel

SKU: 234
Details
Details
UNC Blind Bolt Steel
d1d2BAd3C
5/16"0.3750 0.4060.81300.7500 1.063
3/8"0.43750.62501.15601.00001.3130
3/8"0.43752.06303.65601.00001.3130
1/2"0.56250.50001.18801.12501.3750
5/8"0.68750.68801.56301.56301.8130
3/4"0.81251.50003.25001.81302.2500
7/8"0.93752.00003.18801.87502.3130
1."1.06250.87502.37502.12502.4060
Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand Term-
Diameter 5/16",3/8",3/8",1/2",5/8",3/4",7/8",1."
LengthVARIOUS