| D | ds f7 | dc max | dk min | h min | k | b |
|---|
| M5 | 5.0000 | 9.1000 | 7.7700 | 1.0000 | 6.5000 | 9.0000 |
| M6 | 6.0000 | 10.6000 | 8.9100 | 1.2000 | 7.5000 | 10.0000 |
| M8 | 8.0000 | 13.6000 | 11.1800 | 1.6000 | 8.6000 | 11.5000 |
| M10 | 10.0000 | 16.7000 | 13.4200 | 2.0000 | 10.1000 | 14.5000 |
| M12 | 12.0000 | 19.9000 | 15.6500 | 2.2000 | 11.4000 | 16.0000 |
Additional Info
Additional Info| Weight | 0.0000 |
|---|
| Material | Stainless-Steel-A4 |
|---|
| Standard Number | DIN65438 |
|---|
| Second Standard | - |
|---|
| Drive | 12point |
|---|
| Head | Flange |
|---|
| American Generic Brand Term | FERRY |
|---|
| Diameter | M5,M6,M8,M10,M12 |
|---|
| Length | 16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80 |
|---|