Metric Fine Hexagon Head Bolt Grade-8.8 DIN960

SKU: 23
Details
Details
Metric Fine Hexagon Head Bolt Grade-8.8 DIN960
dkes
M6(0.75p)4.000011.050010.0000
M8(1.00p)5.300014.380013.0000
M10(1.00p)6.400018.900017.0000
M10(1.25P)6.400018.900017.0000
M12(1.25p)7.500021.100019.0000
M12(1.50p)7.500021.100019.0000
M14(1.5p)8.800024.490022.0000
M16(1.5p)10.000026.750024.0000
M18(1.5P)11.5000 27.0000
M20(1.5P)12.5000 30.0000
M24(2.0P)15.0000 36.0000
M27(2.00P)17.0000 41.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard NumberDIN960
Second StandardISO8765
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP
Diameter M6(0.75p),M8(1.00p),M10(1.00p),M10(1.25P),M12(1.25p),M12(1.50p),M14(1.5p),M16(1.5p),M18(1.5P),M20(1.5P),M24(2.0P),M27(2.00P)
Length10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100