Metric Coarse Hexagon Head Bolt Grade-8.8 DIN931

SKU: 1
Details
Details

 

 D   k nom  k Max  Min   s max  s min   e nom  e Max  Min  shank Max  shank Min 
 M1.6          1.10       1.225       0.975         3.20         3.08         3.41         3.70         3.48         1.60         1.46
 M2          1.40       1.525       1.275         4.00         3.88         4.32         4.60         4.38         2.00         1.86
 M2.5          1.70       1.825       1.575         5.00         4.88         5.45         5.80         5.51         2.50         2.23
 M3          2.00       2.125       1.875         5.50         5.38         6.01         6.40         6.08         3.00         2.86
 M3.5          2.40           6.00          6.58    
 M4          2.80       2.925       2.675         7.00         6.85         7.66         8.10         7.74         4.00         3.82
 M5          3.50       3.650       3.350         8.00         7.85         8.79         9.20         8.87         5.00         4.82
 M6          4.00       4.150       3.850       10.00         9.78       11.05       11.50       11.05         6.00         5.82
 M7          4.80         11.00        12.12    
 M8          5.30       5.650       5.350       13.00       12.73       14.38       15.00       14.38         8.00         7.78
 M10          6.40       7.180       6.820       17.00       16.73       18.90       19.60       18.90       10.00         9.78
 M12          7.50       8.180       7.820       19.00       18.67       21.10       21.90       21.10       12.00       11.73
 M14          8.80       9.180       8.820       22.00       21.67       24.49       25.40       24.49       14.00       13.73
 M16        10.00    10.180       9.820       24.00       23.67       26.75       27.70       26.75       16.00       15.73
 M18        11.50    12.215    11.785       27.00       26.67       30.14       31.20       30.14       18.00       17.73
 M20        12.50    13.215    12.785       30.00       29.67       33.53       34.60       33.53       20.00       19.67
 M22        14.00    14.215    13.785       32.00       31.61       35.72       36.90       35.72       22.00       21.67
 M24        15.00    15.215    14.785       36.00       35.38       39.98       41.60       39.98       24.00       23.67
 M27        17.00    17.215    16.785       41.00       40.38       45.20       47.30       45.63       27.00       26.67
 M30        18.70    19.260    18.740       46.00       45.38       50.85       53.10       51.28       30.00       29.67
 M33        21.00    21.260    20.740       50.00       49.38       55.37       57.70       55.80       33.00       32.61
 M36        22.50    23.260    22.740       55.00       54.26       60.79       63.50       61.31       36.00       35.61
 M39        25.00    25.260    24.740       60.00       59.26       66.40       69.30       66.96       39.00       38.61
 M42        26.00    26.260    25.740       65.00       64.26       71.30       75.10       72.61       42.00       41.61
 M45        28.00    28.260    27.740       70.00       69.26       76.95       80.80       78.26       45.00       44.61
 M48        30.00    30.260    29.740       75.00       74.26       82.60       86.60       83.91       48.00       47.61
 M52        33.00    33.210    32.690       80.00       79.26       88.30       92.40       89.56       52.00       51.54
 M56        35.00    35.310    34.690       85.00       84.13       93.63       98.10       95.07       56.00       55.54
 M60        38.00    38.310    37.690       90.00       89.13       99.35    103.90    100.72       60.00       59.54
 M64        40.00    40.310    39.690       95.00       94.13    104.98    109.70    106.37       64.00       63.54
 M68        43.00    43.310    42.690    100.00       99.13    110.50    115.50    112.02       68.00       67.54
 M72        45.00      105.00    102.80    116.03          71.26
 M76        48.00      110.00    107.80    121.55          75.26
 M80        50.00      115.00     127.30          79.26
 M90        57.00      130.00     144.00          89.13
 M100        63.00      145.00     161.00          99.13
 M110        69.00      155.00     171.28       109.13
 M125        79.00      180.00     198.90       124.00
 M140        88.00      200.00     221.00       139.00
 M160     100.00      230.00     254.15       159.00

Metric Coarse Hexagon Head Bolt class 8.8 DIN 931

Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard NumberDIN931
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP
Diameter M1.6,M2,M2.5,M3,M3.5,M4,M5,M6,M7,M8,M10,M12,M14,M16,M18,M20,M22,M24,M27,M30,M33,M36,M39,M42,M45,M48,M52,M56,M60,M64,M68,M72,M76,M80,M90,M100,M110,M125,M140,M160
Length6,8,10,12,14,16,18,20,22,24,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200,210,220,230,240,250,260,270,280,300,320,340,350,360,380,400,420,440,460,480,500