Metric Coarse Verbu Ripp Hexagon Flange Bolt Serrated Underhead Grade-8.8

SKU: 2426
Details
Details
Metric Coarse Verbu Ripp Hexagon Flange Bolt Serrated Underhead Grade-8.8
dsekgdc
M58.00008.87004.30001.700011.2000
M610.000011.05005.50002.300014.2500
M813.000014.38007.00003.000018.2500
M1015.000016.64007.90003.600021.0000
M1217.000018.90008.70004.400024.0000
M1622.000024.490011.20006.700031.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-8.8
Standard Number.
Second StandardVERBUSRIPP
DriveHexagon
HeadFlange
American Generic Brand Term-
Diameter M5,M6,M8,M10,M12,M16
Length8,10,12,16,20,25,30,35,40,50,60,70