Metric Coarse Cup Head Square Neck Bolt Grade-10.9 DIN11015

SKU: 91
Details
Details
Metric Coarse Cup Head Square Neck Bolt Grade-10.9 DIN11015
dbckse
M822.000020.00004.50008.00003.5000
M1026.000024.00005.500010.00004.5000
M1230.000030.00007.000012.00005.5000
M1638.000040.00009.000016.00006.0000
M2046.000046.000010.000020.00008.0000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberDIN11015
Second Standard-
DriveNon
HeadCup
American Generic Brand Term-
Diameter M8,M10,M12,M16,M20
Length20,25,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,120,140,160