Metric Coarse Cup Head Nib Bolt with DIN555 Nut Grade-4.6 DIN607

SKU: 92
Details
Details
Metric Coarse Cup Head Nib Bolt with DIN555 Nut Grade-4.6 DIN607
Ddkkbg
M816.55006.380022.00003.0000
M1019.65007.450026.00003.2000
M1224.65009.650030.00003.6000
M1630.650011.750038.00004.2000
Additional Info
Additional Info
Weight0.0000
MaterialGrade-4.6
Standard NumberDIN607
Second Standard-
DriveNib
HeadCup
American Generic Brand TermROUND
Diameter M8,M10,M12,M16
Length20,25,26,28,30,35,40,45,50,55,60,65,70,75,80,85,90,95,100,120,140,160