UNC Rib Neck Carriage Bolt SAE-5(8.8) B18.5

SKU: 85
Details
Details

UNC Rib Neck Carriage Bolt SAE-5 (8.8) B18.5

 

SizeNo.101/4”5/16”3/8”7/16”1/2”5/8”3/4”
Dec0.190.250.3130.3750.4380.50.6250.75
B max0.1990.260.3240.3880.4520.5150.6420.768
B min0.1820.2370.2980.360.4210.4830.6050.729
W max 0.4690.5940.7190.8440.9691.0941.3441.594
W min0.4380.5630.6880.7820.9071.0321.2191.469
H max0.1140.1450.1760.2080.2390.270.3440.406
H min0.0940.1250.1560.1880.2190.250.3130.375
7/8" or shorter head to ribs0.0310.0310.0310.0310.0310.0310.0940.094
1" and longer head to ribs0.0630.0630.0630.0630.0630.0630.0940.094
number of ribs910121214161922
V min0.210.2740.340.4050.470.5340.660.785
D 7/8" or shorter0.250.250.250.250.250.250.3130.313
D 1" and 1.1/8"0.4070.4070.4070.4070.4070.4070.4380.438
D 1.1/4 or longer0.5940.5940.5940.5940.5940.5940.6250.625
R0.0310.0310.0310.0310.0310.0310.0620.062

 

 

Additional Info
Additional Info
Weight0.0000
MaterialSAE-5(8.8)
Standard NumberB18.5
Second Standard-
DriveSpline
HeadCup
American Generic Brand Term RIBBED,
Diameter No10,1/4",5/16",3/8",7/16",1/2",9/16",5/8",3/4"
Length1/2",5/8",3/4",7/8",1.",1.1/8",1.1/4",1.3/8",1.1/2",1.5/8",1.3/4",2.",2.1/4",2.3/8",2.1/2",2.3/4",3.",3.1/4",3.1/2",3.3/4",4.",4.1/4",4.1/2",4.3/4",5.",5.1/4",5.1/2",5.3/4",6."