BSW Whitworth Dynamo Eye Bolt Forged with Shoulder Collar Steel BS4278T6

SKU: 143
Details
Details

 

dckefhL
3/8”0.66930.19690.86610.35431.06300.7087
1/2”0.90550.23621.14170.43311.33860.9055
5/8”1.10240.31501.37800.55121.65351.1024
3/4”1.25980.35431.57480.59061.85041.2598
7/8”1.37800.39371.73230.66932.08661.3780
1”1.57480.47242.00790.74802.36221.5748
1.1/4”2.00790.55122.51970.94492.99212.0079
1.1/2”2.48030.70873.11021.18113.74022.4803
1.3/4”3.11020.86613.89761.45674.64573.1102
2”3.50391.02364.40941.65355.27563.5039

 

BSW Whitworth Dynamo Eye Bolt Forged with Shoulder Collar Steel BS4278T6

BSW Whitworth Dynamo Eye Bolt Forged with Shoulder Collar Steel BS 4278 T6 table six

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard NumberBS4278T6
Second Standard-
DriveNon
HeadEYE
American Generic Brand TermDYNAMO
Diameter 3/8",1/2",5/8",3/4",1.",1.1/4",1.1/2",1.3/4",2."