UNC Wing Nut American Type D1 Stamped Steel B18.6.9D1
SKU:
1139
Details
Details
UNC Wing Nut American Type D1 Stamped Steel B18.6.9D1
d | A | B | C | D | E | G | H |
---|
No. 8 | 0.7800 | 0.4000 | 0.1800 | 0.2500 | 0.4100 | 0.0800 | 0.1200 |
No. 10 | 0.9100 | 0.4700 | 0.2100 | 0.3400 | 0.5300 | 0.1000 | 0.1200 |
No. 12 | 1.0900 | 0.4700 | 0.2100 | 0.3400 | 0.5300 | 0.1000 | 0.1200 |
1/4" | 1.1100 | 0.5000 | 0.2500 | 0.3400 | 0.6200 | 0.1100 | 0.1200 |
5/16" | 1.3000 | 0.5900 | 0.3000 | 0.4600 | 0.7300 | 0.1400 | 0.1800 |
3/8" | 1.4100 | 0.6700 | 0.3400 | 0.6900 | 0.8300 | 0.1600 | 0.1800 |
Additional Info
Additional InfoWeight | 0.0000 |
---|
Material | STEEL |
---|
Standard Number | B18.6.9D1 |
---|
Second Standard | - |
---|
Drive | Wing |
---|
Head | NON |
---|
American Generic Brand Term | THUMB |
---|
Diameter | No.8,No.10,No.12,1/4",5/16",3/8" |
---|
Length | NON |
---|