Metric Coarse Structural Hexagon Full Nut HSFG Class-8 BS EN15048 Non Preload

SKU: 2653
Details
Details

 

Metric Coarse Structural Hexagon Full Nut HSFG Class-8 BS EN15048


 

 

dM12M16M20M24M30M36
da max       13.00       17.30       21.60       25.90       32.40       38.90
da min       12.00       16.00       20.00       24.00       30.00       36.00
dw min       16.60       22.50       27.70       33.30       42.80       51.10
e min       20.03       26.75       32.95       39.55       50.85       60.79
m max       10.80       14.80       18.00       21.50       25.60       31.00
m min       10.37       14.10       16.90       20.20       24.30       29.40
s max       18.00       24.00       30.00       36.00       46.00       55.00
s min       17.73       23.67       29.16       35.00       45.00       53.80


 


Metric Coarse Structural Hexagon Full Nut H.S.F.G Class 8 BS EN5048

Additional Info
Additional Info
Weight0.0000
MaterialClass-10
Standard NumberEN143993
Second Standard-
DriveHexagon
HeadNON
American Generic Brand TermHIGHSTRENGTHFRICTIONGRIPNUT
Diameter M12,M16,M20,M22,M24,M27,M30,M36
LengthNON