Metric Hardened Chamfered Flat Washer HSFG Hardened Steel BS EN 14399-6

SKU: 2587
Details
Details

Metric Hardened Chamfered Flat Washer HSFG Hardened Steel BS EN 14399-6

 

 

dM16M20M22M24M27M30M36

d1 min

 17.00 21.00 23.00  25.00  28.00  31.00  37.00

d1max

 17.27 21.33 23.33  25.33  28.52  31.62  37.62

d2 min

 29.48 36.38 38.38  43.38  49.00  54.80  64.80

d2max

 30.00 37.00 39.00  44.00  50.00  56.00  66.00

h nom

   4.00   4.00   4.00    4.00    5.00    5.00    6.00

h min

   3.70   3.70    3.70    3.70    4.40    4.40    5.40

h max

   4.30   4.30    4.30    4.30    5.60    5.60   6.60

e min

   0.75   0.75     0.75     0.75     1.00    1.00   1.25

e max

   1.50   1.50     1.50     1.50     2.00     2.00   2.50

c min

   1.60   2.00     2.00     2.00     2.50    2.50   2.50

c max

   1.90   2.50     2.50     2.50      3.00    3.00   3.00

 

 

Metric Hardened Chamfered Flat Washer High Strength Friction Grip Hardened Steel BS EN 14399 6

 



Additional Info
Additional Info
Weight0.0000
MaterialHARDENED STEEL
Standard NumberDIN6916
Second Standard-
DriveNon
HeadNON
American Generic Brand TermHIGHSTRENGTHFRICTIONGRIPWASHER
Diameter M12,M16,M20,M22,M24,M27,M30,M36