Metric Coarse High Strength Friction Grip H.S.F.G Grade-10.9 EN14399-4


 

d1M12M16M20M22M24M27M30M36
c max.         0.80         0.80         0.80         0.80         0.80         0.80         0.80         0.80
c min.         0.40         0.40         0.40         0.40         0.40         0.40         0.40         0.40
h max.       12.70       16.70       20.84       22.84       24.84       27.84       30.84       37.00
h min.       11.30       15.30       19.16       21.16       23.16       26.16       29.16       35.00
k max.         7.95       10.75       13.40       14.90       15.90       17.90       19.75       23.55
k min.         7.05         9.25       11.60       13.10       14.10       16.10       17.65       21.45
s max       22.00       27.00       32.00       36.00       41.00       46.00       50.00       60.00
s min.       21.16       26.16       31.00       35.00       40.00       45.00       49.00       58.80
e min.       23.91       29.56       35.03       39.55       45.20       50.85       55.37       66.44
ds min       11.30       15.30       19.16       21.16       23.16       26.16       29.16       35.00
ds max       12.70       16.70       20.84       22.84       24.84       27.84       30.84       37.00
dw min       20.10       24.90       29.50       33.30       38.00       42.80       46.60       55.90
da max       15.20       19.20       24.40       26.40       28.40       32.40       35.40       42.40
b <1253038465054606678
b 125-200-44525660667284
b> 200--656973798597

 

Metric Coarse High Strength Friction Grip HSFG class 10.9 EN14399-4High Strength Friction Grip HSFG Grade-110.9 EN 14399 Structural H.S.F.G Bolt class 8.8 EN14399-4 Preload

Additional Info
Additional Info
Weight0.0000
MaterialGrade-10.9
Standard NumberEN143993
Second Standard-
DriveHexagon
HeadHEXAGON
American Generic Brand TermHEXAGONCAP,HIGHSTRENGTHFRICTIONGRIP
Diameter M12,M16,M20,M22,M24,M27,M30,M36
Length35,40,45,50,55,60,65,70,75,80,85,90,95,100,110,120,130,140,150,160,170,180,190,200
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.