ALegs   B                  C  push on force kg  pull off force kg  
1.5mm49.7020.2034kg20kg
2mm49.7020.2037kg20kg
3mm49.7020.20311kg20kg
4mm511.4810.2037kg40kg
5mm611.4810.20312kg40kg
6mm615.2910.25415kg80kg
7mm615.2910.25419kg80kg
8mm615.2910.25422kg80kg
9mm618.4400.30521kg100kg
10mm618.4400.30529kg100kg
11mm618.4400.30542kg100kg
12mm625.0200.40645kg250kg
13mm625.0200.40635kg250kg
14mm628.2450.40625kg250kg
15mm628.2450.40634kg250kg
16mm628.1500.40656kg250kg
17mm628.2450.40649kg250kg
18mm636.5760.40623kg350kg
19mm936.5760.40616kg385kg
20mm936.5760.40627kg350kg
21mm936.5760.40621kg385kg
22mm936.5760.40655kg350kg
23mm938.1760.45771kg350kg
24mm941.3760.50846kg385kg
25mm941.3500.50857kg385kg
  
  

Metric Starlock Washer Uncapped Steel push nut 

Additional Info
Additional Info
Weight0.0000
MaterialSTEEL
Standard Number.
Second StandardBAKERFINNYMORE
Drive-
Head-
American Generic Brand Term-
Diameter0
LengthNON
Reviews
Tags
Tags

Use spaces to separate tags. Use single quotes (') for phrases.