d | Pitch | s | h | m |
---|---|---|---|---|
M5 | 0.8 | 8 | 6.3 | 4.00 |
M6 | 1 | 10 | 8.2 | 4.50 |
M8 | 1.25 | 13 | 10.8 | 6.70 |
M10 | 1.50 | 17 | 12.6 | 8.00 |
M12 | 1.75 | 19 | 16 | 10.60 |
M14 | 2 | 22 | 18 | 12.00 |
M16 | 2 | 24 | 20.6 | 13.5 |
M18 | 2.5 | 27 | 22.5 | 14.5 |
M22 | 2.5 | 32 | 29.8 | 20.5 |
M20 | 2.5 | 30 | 25.5 | 16.9 |
M24 | 3 | 36 | 29.9 | 20.6 |
M27 | 3 | 41 | 33.7 | 24.3 |
M30 | 3.5 | 46 | 37 | 26.6 |
M33 | 3.5 | 50 | 40.5 | 28.8 |
M36 | 4 | 55 | 44.2 | 31.5 |
Metric Coarse Vargal Lock Nut fastener Standard Class grade 8 grade8 abbott jeveka etra kpo gally
Weight | 0.0000 |
---|---|
Material | Class-8 |
Standard Number | . |
Second Standard | VARGAL |
Drive | Hexagon |
Head | NON |
American Generic Brand Term | STIFF, PREVAILING TORQUE |
Diameter | 0 |
Length | NON |